maxxkatt
Forum Supporter
I have used electrolysis to clean a couple of old axe heads. I used a single scrap piece of steel as my positive and clipped the negative on my relic. all worked well.
I am trying to decrease the electrolysis time by putting four pieces of aluminum at North, south, east and west on my bucket for my positive.
will aluminum work or does it have to be iron or steel for your positive?
I am trying to decrease the electrolysis time by putting four pieces of aluminum at North, south, east and west on my bucket for my positive.
will aluminum work or does it have to be iron or steel for your positive?